stress corrosion test 应力腐蚀试验
slow-drawing stress corrosion test 慢应变速率应力腐蚀试验
sulfide stress corrosion cracking test H2S应力腐蚀试验
stress corrosion cracking test 应力腐蚀试验
H2S stress corrosion cracking test H2S应力腐蚀开裂实验
Results After stress-corrosion test, there was no discoloration in the weld zone of the laser-welded cast samples.
不进行应力腐蚀试验的激光焊接铸钛试样作为对照组。
After the integrated analysis of each test result, it is proved that the pipe leakage failure is of stress corrosion damage.
在对各项试验结果进行综合分析之后确认,该管路泄漏失效为应力腐蚀破坏。
In this paper, we raise really available measures through the investigation, analysis, test and research about the stress corrosion cracking of pressure vessel for ammonia refrigerating equipments.
通过对氨制冷压力容器应力腐蚀开裂进行调查、分析、试验和研究,提出切实可行的对策措施。