On the oval or round aggregate,the high-permeable concrete compressive failure process is basically along the thin interface between the pore and cement damage started,extending to four weeks. When the cement and the interface damage to a certain extent,aggregate begins to undermine,then the specimen will suffer loss of load capacity.